+86-755-23202160 | Temper | Annealed | |
|---|---|---|
| Tensile Rm | 100 | ksi (min) |
| Tensile Rm | 690 | MPa (min) |
| R.p. 0.2% Yield | 45 | ksi (min) |
| R.p. 0.2% Yield | 310 | MPa (min) |
| Elongation (2” or 4D gl) | 40 | % (min) |
| Element | Min | Max |
|---|---|---|
| C | - | 0.001 |
| Si | - | 0.1 |
| Mn | - | 0.5 |
| P | - | 0.015 |
| S | - | 0.01 |
| Al | 0.1 | 0.4 |
| Co | - | 0.3 |
| Cr | 22 | 24 |
| Cu | - | 0.5 |
| Fe | - | 1.5 |
| Mo | 15 | 16.5 |
| Ni | Balance | |
| Temper | Annealed | |
|---|---|---|
| Tensile Rm | 100 | ksi (min) |
| Tensile Rm | 690 | MPa (min) |
| R.p. 0.2% Yield | 45 | ksi (min) |
| R.p. 0.2% Yield | 310 | MPa (min) |
| Elongation (2” or 4D gl) | 40 | % (min) |
| Element | Min | Max |
|---|---|---|
| C | - | 0.001 |
| Si | - | 0.1 |
| Mn | - | 0.5 |
| P | - | 0.015 |
| S | - | 0.01 |
| Al | 0.1 | 0.4 |
| Co | - | 0.3 |
| Cr | 22 | 24 |
| Cu | - | 0.5 |
| Fe | - | 1.5 |
| Mo | 15 | 16.5 |
| Ni | Balance | |